»ó¼¼ ¼³¸í
¡Ü BI-XDC´Â º¸Á¤¾øÀÌ ÀÔµµ¸¦ ÃøÁ¤ÇÒ ¼ö ÀÖ´Â ±¤µð½ºÅ© ¿ø½ÉºÐ¸® ÀÔµµºÐ¼®±â ÀÔ´Ï´Ù. ¶ÇÇÑ X-ray¸¦ »ç¿ëÇÏ¿© ³ôÀº ±¼Àý·üÀ» °¡Áø ½Ã·á ÃøÁ¤¿¡ ÀûÇÕ´Ï´Ù.
(¿ø¼Ò¹øÈ£ 20 ¹ø ÀÌ»óÀÇ ¹°ÁúÀ» ÃøÁ¤¿¡ ÀûÇÕÇÑ Àåºñ ÀÔ´Ï´Ù.)
¡Ü ÃÖ¼Ò15% Â÷À̸¦ º¸ÀÌ´Â °í³óµµ ½Ã·áÀÇ Å©±â¸¦ ºÐ¼®ÇÏ°í, ºÐÆ÷¸¦ Á¤·®È­ ÇÒ ¼ö ÀÖ½À´Ï´Ù.
¡Ü ±¤»ê¶õ º¸Á¤¾øÀÌ, ºÎÇÇ/Áú·® ºÐ»êµµ¸¦ ¹Ù·Î ÃøÁ¤ÇÕ´Ï´Ù.

ÀÀ¿ëºÐ¾ß

• »êÈ­¹° ³ª³ëÀÔÀÚ
• ±Ý¼Ó»êÈ­¹°, ±Ý¼ÓºÐ¸»
• ¾Ë·ç¹Ì³ª, ¾Ë·ç¹Ì³ª ¼¼¶ó¹Í
• »êȭƼ³ª´½(TiO2) ÇöŹ¾×
• Áö¸£ÄÚ´Ï¾Æ ³ª³ëÀÔÀÚ
• Super-paramagnetic iron oxide nanoparticles (SPION)
• ÅÖ½ºÅÙ ³ª³ëÀÔÀÚ
• ¿¬¸¶Á¦
• ³ª³ë ¼¼¶ó¹Í ÀÔÀÚ
• ÀÌ»êÈ­¼¼·ý ³ª³ëÀÔÀÚ
• ±Ý¼Ó ÇÁÅ»·Î½Ã¾Æ´Ñ ³ª³ëº¹ÇÕ¼ÒÀç
• źȭ±Ô¼Ò(Silicon Carbide)
• ÁúÈ­±Ô¼Ò(Silicon Nitride) Å©±â
• ÄɽºÆà ÀÔÀÚ Å©±â
• ±¤¹°
• Ŭ·¹ÀÌ
»ó¼¼ ±Ô°Ý

Size Range

0.01-100 microns, depends on particle and liquid density and liquid viscosity

Centrifuge Speed

500-6000 rpm, +/-0.01%, high speed disc available see options

Disc

PMMA construction, 10-30 mL volume, solvent resistant disc available see options

Scanning Speed

0.05-10 mm/min, 1 mm/min typical

Measurement Time

3-30 min, typically 8 min/decade in particle diameter,

Data System

High-performance Windows¢â system with color printer. Contact factory for latest specifications

Software

Written for Windows¢â, control, archiving and data analysis,

Power Requirements

100/115/240 VAC, 50/60 Hz, 300 Watts,

Dimensions

230(H) x 460(W) x 600(D), mm

Weight

35 kgs

Certifications

CE Marked